ASTM WK98768
When UNS N08800 was transferred from ASTM SB-564/SB-564M to ASTM A182/A182M, A403/A403M, and A965/A965M, the tensile values were erroneously transcribed in the Mechanical Properties Tables as Tensile Strength and Yield Strength, min, ksi[MPa] 65 [450] 25 [170] for A812/A182M, 65 [520] 25 [205] for A403/A403M and 65n [450] 25 [170] for A965/A965M instead of 75 [515] 30 [205] as reflected in the source document adjusted for the rounding practices of A01. This error was discovered as ASME is attempting to transfer the stress allowables in ASME Section II Part D from the Nonferrous to Ferrous Tables. All other product form currently require 75 [515] 30 [205]. Correction is urgent to remove the discrepancies. This WK revises these values for A182/A182M.