Revision of E2899-19e1 Standard Test Method for Measurement of Initiation Toughness in Surface Cracks Under Tension and Bending

Rationale

E2899 (no change)
3.2.7 notch height, h [L]—the distance between the parallel faces of the machined notch prior to specimen deformation (Fig. 6).