MANUAL Published: 01 January 1999
MNL10338M

Chapter 16 Importance of Constraint and Loading-The Ingram Barge

Source

THIS CHAPTER DISCUSSES the brittle fracture of the Ingram Barge which occurred in 1972. This ship had a notch toughness level of about 55 ft-lb at the service temperature, well above what would generally be considered adequate to prevent a brittle fracture. However, in this case, the three-dimensional constraint based on the design was such that the principle stresses, σ1, σ2, and σ3, were relatively high in tension. This triaxial state of tensile stresses prevented the development of significant shear stresses at the fracture origin. Thus, as would be concluded from strength of materials principles, brittle fracture could occur when the three principal stress components are large.

Author Information

Price: $25.00
Contact Sales
Related
Reprints and Permissions
Reprints and copyright permissions can be requested through the
Copyright Clearance Center
Details
Developed by Committee: E08
Pages: 428–437
DOI: 10.1520/MNL10338M
ISBN-EB: 978-0-8031-4541-2