Abstract

The modified wedge-opening-load (WOL) specimen introduced by Novak and Rolfe is now commonly employed to establish crack growth rate and threshold of stress corrosion cracking KIscc data. The present paper is concerned with the stress intensity factor solution for this specimen with 10% side grooving. Finite element and experimental compliance studies were undertaken to define the stress intensity factor solution in terms of crack mouth opening displacement. The analytical and experimental results obtained were found to be in excellent agreement. The results also verify the use of Wilson's finite element stress intensity calibration of the T-type WOL specimen when the effect of the side grooves is accounted for.

Author Information

LeFort, P
Materials and Processes Laboratory, General Electric Co., Schenectady, N.Y.
Mowbray, DF
Materials and Processes Laboratory, General Electric Co., Schenectady, N.Y.
Pages: 6
Price: $25.00
Related
Reprints and Permissions
Reprints and copyright permissions can be requested through the
Copyright Clearance Center
Details
Stock #: JTE10929J
ISSN: 0090-3973
DOI: 10.1520/JTE10929J