Abstract

Stress relaxation data on commercially available copper-beryllium alloy 172 are presented. Test samples were subjected to strains of up to 2% and temperatures from 25 to 181°C. The data show that a high degree of relaxation occurs at higher temperatures and relaxation was found to be independent of the initial stress levels. Time-temperature plots of stress relaxation are presented for designing accelerated relaxation tests on the copper-beryllium alloy tested. The material in the tested condition is generally not used in spring applications and thus results of Austen which compare stress relaxation characteristics of copper-beryllium alloy 172 in the aged and unaged conditions are also presented.

Author Information

Goel, RP
Bell Telephone Laboratories, Inc., Columbus, Ohio
Pages: 6
Price: $25.00
Related
Reprints and Permissions
Reprints and copyright permissions can be requested through the
Copyright Clearance Center
Details
Stock #: JTE10134J
ISSN: 0090-3973
DOI: 10.1520/JTE10134J