Standard Active Last Updated: Mar 15, 2023 Track Document
ASTM D4273-23

Standard Test Method for Polyurethane Raw Materials: Determination of Primary Hydroxyl Content of Polyether Polyols

Standard Test Method for Polyurethane Raw Materials: Determination of Primary Hydroxyl Content of Polyether Polyols D4273-23 ASTM|D4273-23|en-US Standard Test Method for Polyurethane Raw Materials: Determination of Primary Hydroxyl Content of Polyether Polyols Standard new BOS Vol. 08.02 Committee D20
$ 69.00 In stock

Significance and Use

5.1 The primary hydroxyl content provides information about the relative reactivities of polyols in the urethane forming reaction with isocyanates.

Scope

1.1 Carbon-13 Nuclear Magnetic Resonance Spectroscopy (13C NMR) measures the primary hydroxyl content of ethylene oxide (EO)-propylene oxide (PO) polyether polyols used in preparing flexible polyurethane foams. This method is best suited for polyether polyols with primary hydroxyl contents of 10 to 90 %.

1.2 The values stated in SI units are to be regarded as standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

Note 1: There is no known ISO equivalent to this standard.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Price:
Contact Sales
Related
Reprints and Permissions
Reprints and copyright permissions can be requested through the
Copyright Clearance Center
Details
Book of Standards Volume: 08.02
Developed by Subcommittee: D20.22
Pages: 7
DOI: 10.1520/D4273-23
ICS Code: 83.080.20