    Effect of Cenosphere Size and Volume Fraction on the Microstructure and Deformation Behavior of Ti-Cenosphere Syntactic Foam Made Through Powder Metallurgy Route

    (Received 13 October 2015; accepted 24 August 2016)

    Published Online: 2016

    CODEN: MPCOAD

      Format Pages Price  
    PDF (5.65 MB) 23 $25   ADD TO CART

    Cite this document

    X Add email address send
    X
      .RIS For RefWorks, EndNote, ProCite, Reference Manager, Zoteo, and many others.   .DOCX For Microsoft Word



    Abstract

    An attempt was made for making Titanium–cenosphere metal syntactic foams with varying relative densities, using different cenosphere sizes and volume fractions. Cold compaction of Ti and cenosphere powder mix was carried out at a pressure of 75 MPa, followed by sintering at 1100°C for 2 h. The sintered foam samples were characterized in terms of microstructure, primarily to observe the extent of cenosphere crushing, distribution of cenosphere, and extent of sintering. Uniform distribution of cenosphere with some extent of cenosphere crushing has been observed within the Ti matrix. XRD and EDX analysis confirms the oxidation of Ti particles to a small extent and also the entrapment of crushed cenosphere shells within the matrix, which makes the foam stronger but brittle in nature. The plateau stress, energy absorption, and modulus of these foams vary with the cenosphere size and volume fraction. Foams made with finer size cenosphere exhibits higher plateau stress and higher energy absorption for a fixed cenosphere volume fraction and at a constant foam density. Crushing of cenosphere, while compaction causes an increased density of the foam as compared to the theoretical value. As a consequence, the foam with higher cenosphere volume fraction or with coarser cenosphere size exhibited marginally higher strength and energy absorption. The variation in deformation mechanism as a function of cenosphere size and volume fraction was examined. These foams exhibited considerably higher strength and stiffness than the conventional foam and demonstrate the possibility of using them for biomedical and engineering applications.


    Author Information:

    Pandey, S.
    CSIR-Advanced Materials and Processes Research Inst., Bhopal,

    Venkat, A. N. C.
    CSIR-Advanced Materials and Processes Research Inst., Bhopal,

    Mondal, D. P.
    CSIR-Advanced Materials and Processes Research Inst., Bhopal,

    Majumdar, J. D.
    Indian Inst. of Technology, Kharagpur,

    Jha, A. K.
    CSIR-Advanced Materials and Processes Research Inst., Bhopal,

    Rao, H.
    Peoples College of Medical Science and Research, Bhopal,

    Kumar, H.
    Indian Inst. of Science Education and Research, Bhopal,


    Stock #: MPC20160021

    ISSN:2165-3992

    DOI: 10.1520/MPC20160021

    Author
    Title Effect of Cenosphere Size and Volume Fraction on the Microstructure and Deformation Behavior of Ti-Cenosphere Syntactic Foam Made Through Powder Metallurgy Route
    Symposium ,
    Committee D30