ASTM D2807-93(1998)

    Standard Test Method for Chromic Oxide in Leather (Perchloric Acid Oxidation)


      Format Pages Price  
    PDF 3 $52.00   ADD TO CART


    1. Scope

    1.1 This test method covers the determination of chromic oxide in leathers that have been partly or completely tanned with chromium compounds. In general the samples will contain between 1 and 5% chromium, calculated as chromic oxide.

    1.2 This standard does not purport to address the safety problems, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. See Section 7 for specific safety hazards.


    2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.

    ASTM Standards

    D2617 Test Method for Total Ash in Leather

    D2813 Practice for Sampling Leather for Physical and Chemical Tests

    D2868 Test Method for Nitrogen Content (Kjeldahl) and Hide Substance Content of Leather, Wet Blue and Wet White

    D3495 Test Method for Hexane Extraction of Leather

    D3790 Test Method for Volatile Matter (Moisture) of Leather by Oven Drying


    Referencing This Standard
    Link Here
    Link to Active (This link will always route to the current Active version of the standard.)

    DOI: 10.1520/D2807-93R98

    Citation Format

    ASTM D2807-93(1998), Standard Test Method for Chromic Oxide in Leather (Perchloric Acid Oxidation), ASTM International, West Conshohocken, PA, 1998, www.astm.org