12Cr Steels



Pages: 4    Published: Jan 1956


Download this paper for $25 PDF (160K)          View License Agreement
        Click here to download the complete source publication for $55 PDF (2.0M)


Source: STP187-EB


Abstract

Most of the data are for material finish rolled at 1450 F and then tempered. Two sets of results indicate a small effect from finishing size. The molybdenum-bearing materials tended to average slightly higher in relaxation strength than the molybdenum-free alloys.