STP160

    Haynes Alloy No. 25 (L-605)

    Published: Jan 1954


      Format Pages Price  
    PDF Version (344K) 10 $25   ADD TO CART
    Complete Source PDF (5.4M) 10 $55   ADD TO CART


    Abstract

    The recommended heat treatment for Haynes Alloy No. 25 is to anneal or solution heat treat at 2200 F and air cool. Optimum properties are developed by annealing for about 10 min at 2225 F, followed by rapid air cooling. It requires no aging.