SEDL / Journals / Cement, Concrete and Aggregates (CCA) / Citation Page


Volume 26, Issue 2 (December 2004)

ISSN: 0149-6123
CODEN: CCAGPD
Page Count: 5


Effect of Finishing Practices on Performance of Concrete Containing Slag and Fly Ash as Measured by ASTM C 672 Resistance to Deicer Scaling Tests
Taylor, PC
Construction Technology Laboratory, IL

Jennings, VA
Construction Technology Laboratory, IL

Morrison, W
Construction Technology Laboratory, IL

(Received 23 December 2003; accepted 2 July 2004)

Abstract

The test method was developed to evaluate portland cement systems with different air contents, and for the purpose of determining whether the apparent poor performance of concretes containing supplementary cementing materials in the ASTM C 672 deicer scaling test can be attributed to differences in finishing effort or timing of finishing, or both.



Keywords:
freeze-thaw, supplementary cementing materials, fly ash, slag, ASTM C 672, finishing, bleed, set time

Paper ID: CCA11923
DOI: 10.1520/CCA11923
ASTM International is a member of CrossRef.

Author Title Effect of Finishing Practices on Performance of Concrete Containing Slag and Fly Ash as Measured by ASTM C 672 Resistance to Deicer Scaling Tests Symposium , 0000-00-00 Committee C01