1. Rationale
C836 sets a minimum value for adhesion in peel as measured by C794. A recent change in C794 makes it unsuitable for use with C836 without modification. Alternatively a different ASTM adhesion test will be referenced.
Keywords
crack bridging; membrane; waterproofing; Weight loss; Accelerated aging/testing--elastomeric sealants; Adhesion-in-peel; Building materials/applications--specifications; Crack bridging; Decks--specifications; Film; Elastomeric waterproofing membranes--specifications; Extensibility; Flexibility--roofing/waterproofing materials; Hardness tests; Roofing membranes--specifications; Sealants--specifications; Temperature tests--building materials; Thickness; Waterproofing materials/applications ;