Withdrawn Rationale:

This test method covers accelerated procedures for simultaneously determining comparative characteristics of coating systems applied to steep pipe exterior for the purpose of preventing or mitigating corrosion that may occur in underground service where the pipe will be in contact with natural soils and will receive cathodic protection. They are intended for use with samples of coated pipe taken from commercial production and are applicable to such samples when the coating is characterized by function as an electrical barrier.

Formerly under the jurisdiction of Committee D01 on Paint and Related Coatings, Materials, and Applications, this test method was withdrawn in March 2007 in accordance with section 10.5.3.1 of the Regulations Governing ASTM Technical Committees, which requires that standards shall be updated by the end of the eighth year since the last approval date.


1. Scope

1.1 This test method covers accelerated procedures for simultaneously determining comparative characteristics of coating systems applied to steep pipe exterior for the purpose of preventing or mitigating corrosion that may occur in underground service where the pipe will be in contact with natural soils and will receive cathodic protection. They are intended for use with samples of coated pipe taken from commercial production and are applicable to such samples when the coating is characterized by function as an electrical barrier.

1.2 This test method is intended to facilitate testing of coatings where the test cell is cemented to the surface of the coated pipe specimen. This is appropriate when it is impractical to submerge or immerse the test specimen as required by Test Methods G8, G42, or G80. Coating sample configuration such as flat plate and small diameter pipe may be used, provided that the test procedure remains unchanged.

1.3 This test method allows options that must be identified in the report.

1.4 This standard does not purport to address all of the safety problems, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.

ASTM Standards

G8 Test Methods for Cathodic Disbonding of Pipeline Coatings
G12 Test Method for Nondestructive Measurement of Film Thickness of Pipeline Coatings on Steel
G42 Test Method for Cathodic Disbonding of Pipeline Coatings Subjected to Elevated Temperatures
G62 Test Methods for Holiday Detection in Pipeline Coatings
G80 Test Method for Specific Cathodic Disbonding of Pipeline Coatings


Index Terms

anode; attached cell; cathodic; disbondment; electrical stress; electrolyte; salt bridge;



DOI: 10.1520/G0095-87R98E01

ASTM International is a member of CrossRef.


Citing ASTM Standards

[Back to Top]

Standards Tracker

Standards Subscriptions


Users also bought:
G8
A370
G95 G95 G95 G95 G95 G95 G95 G95 G95 G95