ASTM A732 / A732M - 14 Standard Specification for Castings, Investment, Carbon and Low Alloy Steel for General Application, and Cobalt Alloy for High Strength at Elevated Temperatures


    Citing ASTM Standards Citation data is made available by participants in CrossRefs Cited-by Linking service. A comprehensive list of citations to this standard are listed here.

    A395/A395M Standard Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures

    A439 Standard Specification for Austenitic Ductile Iron Castings

    A488/A488M Standard Practice for Steel Castings, Welding, Qualifications of Procedures and Personnel

    A494/A494M Standard Specification for Castings, Nickel and Nickel Alloy

    A536 Standard Specification for Ductile Iron Castings

    A744/A744M Standard Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service

    A890/A890M Standard Specification for Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application

    A897/A897M Standard Specification for Austempered Ductile Iron Castings

    A957/A957M Standard Specification for Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use


    Referenced ASTM Standards The documents listed below are referenced within the subject standard but are not provided as part of the standard.

    A941 Terminology Relating to Steel, Stainless Steel, Related Alloys, and Ferroalloys

    A957/A957M Specification for Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use

    A997 Practice for Investment Castings, Surface Acceptance Standards, Visual Examination

    E21 Test Methods for Elevated Temperature Tension Tests of Metallic Materials

    E139 Test Methods for Conducting Creep, Creep-Rupture, and Stress-Rupture Tests of Metallic Materials