ASTM A426 / A426M - 13 Standard Specification for Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service


    Citing ASTM Standards Citation data is made available by participants in CrossRefs Cited-by Linking service. A comprehensive list of citations to this standard are listed here.

    A999/A999M Standard Specification for General Requirements for Alloy and Stainless Steel Pipe


    Referenced ASTM Standards The documents listed below are referenced within the subject standard but are not provided as part of the standard.

    A370 Test Methods and Definitions for Mechanical Testing of Steel Products

    A609/A609M Practice for Castings, Carbon, Low-Alloy, and Martensitic Stainless Steel, Ultrasonic Examination Thereof

    A941 Terminology Relating to Steel, Stainless Steel, Related Alloys, and Ferroalloys

    A999/A999M Specification for General Requirements for Alloy and Stainless Steel Pipe

    E94 Guide for Radiographic Examination

    E165 Practice for Liquid Penetrant Examination for General Industry

    E186 Reference Radiographs for Heavy-Walled (2 to 412-in. (50.8 to 114-mm)) Steel Castings

    E208 Test Method for Conducting Drop-Weight Test to Determine Nil-Ductility Transition Temperature of Ferritic Steels

    E280 Reference Radiographs for Heavy-Walled (412 to 12-in. (114 to 305-mm)) Steel Castings

    E446 Reference Radiographs for Steel Castings Up to 2 in. (50.8 mm) in Thickness

    E709 Guide for Magnetic Particle Testing