ASTM D5419-95

Standard Test Method for Environmental Stress Crack Resistance (ESCR) of Threaded Plastic Closures

Standard Test Method for Environmental Stress Crack Resistance (ESCR) of Threaded Plastic Closures D5419-95 ASTM|D5419-95|en-US Standard Test Method for Environmental Stress Crack Resistance (ESCR) of Threaded Plastic Closures Standard new BOS Vol. 08.03 Committee D20
$ 75.00 In stock

Scope

1.1 This test method determines the susceptibility of threaded plastic closures to failure due to environmental stress cracking (ESC).

1.2 Threaded plastic closures in use may contact agents that appreciably reduce the stress at which cracks form. Examples of such agents are: soaps, detergents, oils, and liquid bleaches.

1.3 Other major factors that influence environmental stress crack resistance (ESCR) of threaded plastic closures are the closure material(s), closure design, molded-in stress, and applied stress.

1.4 This procedure applies particularly to closures made from plastics based on polypropylene (PP) or polystyrene (PS). It may also apply to other polymers.

1.5 The values stated in SI units are to be regarded as the standard.

1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 8 and Note 2.

Note 1-There are no ISO standards covering the primary subject of this test method.
Price:
Contact Sales
Related
Reprints and Permissions
Reprints and copyright permissions can be requested through the
Copyright Clearance Center
Details
Book of Standards Volume: 08.03
Developed by Subcommittee: D20.20
Pages: 5
DOI: 10.1520/D5419-95
ICS Code: 83.080.20