Standards

ASTM D1076-02


Historical Standard: ASTM D1076-02 Standard Specification for Rubber-Concentrated, Ammonia Preserved, Creamed, and Centrifuged Natural Latex


SUPERSEDED (see Active link, below)


more info 12 pages $ 56.40

Active(view current version of standard) ASTM License Agreement
Other Historical Standards

1. Scope


1.1 This specification covers requirements for first grade concentrated natural rubber latex (see Table 1) of the following types:

Type 1-Centrifuged natural latex preserved with ammonia only or by formaldehyde followed by ammonia.

Type 2-Creamed natural latex preserved with ammonia only or by formaldehyde followed by ammonia.

Type 3-Centrifuged natural latex preserved with low ammonia with other necessary preservatives.

1.2 This specification is not necessarily applicable to latices prepared or preserved by other methods, and shall not be construed as limiting the desirability or usefulness of other types of latices. It does not apply to natural latex sources other than Hevea braziliensisnor to compounded latex concentrates.

1.3 The analytical procedures applicable to the specifications are included and appear in the following order:

Section
Sampling6 and 7
Total Solids8
Dry Rubber Content9
Total Alkalinity10
Viscosity11
Sludge Content12
Coagulum Content13
KOH Number14
pH15
Mechanical Stability16
Copper and Manganese17
Density18-30
Volatile Fatty Acids31-35
Boric Acid36
Dry Films37
Precision for All Test Methods38

1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.


2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.

ASTM Standards

D1278 Test Methods for Rubber from Natural Sources--Chemical Analysis

D4483 Practice for Evaluating Precision for Test Method Standards in the Rubber and Carbon Black Manufacturing Industries

D5712 Test Method for Analysis of Aqueous Extractable Protein in Natural Rubber and Its Products Using the Modified Lowry Method

D6499 Test Method for The Immunological Measurement of Antigenic Protein in Natural Rubber and its Products

E70 Test Method for pH of Aqueous Solutions With the Glass Electrode




Keywords


Acidity, alkalinity, pH--rubber materials/applications; Boric acid content; Coagulum content; Density--rubber; Dry rubber content; Fatty acids content; KOH number; Mechanical stability; Natural rubber (NR) latex--specifications; Rubber--specifications; Sludge; Solids content; Viscosity--rubber; Volatile fatty acids content ;




ICS Code


ICS Number Code 83.040.10 (Latex and raw rubber)