Historical Standard: ASTM B338-10 Standard Specification for Seamless and Welded Titanium and Titanium Alloy Tubes for Condensers and Heat Exchangers


SUPERSEDED (see Active link, below)


more info 8 pages $ 49.20

Active(view current version of standard) ASTM License Agreement
Other Historical Standards

1. Scope

1.1 This specification covers the requirements for 28 grades of titanium and titanium alloy tubing intended for surface condensers, evaporators, and heat exchangers, as follows:

1.1.1 Grade 1Unalloyed titanium,

1.1.2 Grade 2Unalloyed titanium,

1.1.2.1 Grade 2HUnalloyed titanium (Grade 2 with 58 ksi minimum UTS),

1.1.3 Grade 3Unalloyed titanium,

1.1.4 Grade 7Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.4.1 Grade 7HUnalloyed titanium plus 0.12 to 0.25 % palladium (Grade 7 with 58 ksi minimum UTS),

1.1.5 Grade 9Titanium alloy (3 % aluminum, 2.5 % vanadium),

1.1.6 Grade 11Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.7 Grade 12Titanium alloy (0.3 % molybdenum, 0.8 % nickel),

1.1.8 Grade 13Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.9 Grade 14Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.10 Grade 15Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.11 Grade 16Unalloyed titanium plus 0.04 to 0.08 % palladium,

1.1.11.1 Grade 16HUnalloyed titanium plus 0.04 to 0.08 % palladium (Grade 16 with 58 ksi minimum UTS),

1.1.12 Grade 17Unalloyed titanium plus 0.04 to 0.08 % palladium,

1.1.13 Grade 18Titanium alloy (3 % aluminum, 2.5 % vanadium) plus 0.04 to 0.08 % palladium,

1.1.14 Grade 26Unalloyed titanium plus 0.08 to 0.14 % ruthenium,

1.1.14.1 Grade 26HUnalloyed titanium plus 0.08 to 0.14 % ruthenium (Grade 26 with 58 ksi minimum UTS),

1.1.15 Grade 27Unalloyed titanium plus 0.08 to 0.14 % ruthenium,

1.1.16 Grade 28Titanium alloy (3 % aluminum, 2.5 % vanadium) plus 0.08 to 0.14 % ruthenium,

1.1.17 Grade 30Titanium alloy (0.3 % cobalt, 0.05 % palladium),

1.1.18 Grade 31Titanium alloy (0.3 % cobalt, 0.05 % palladium),

1.1.19 Grade 33Titanium alloy (0.4 % nickel, 0.015 % palladium, 0.025 % ruthenium, 0.15 % chromium),

1.1.20 Grade 34Titanium alloy (0.4 % nickel, 0.015 % palladium, 0.025 % ruthenium, 0.15 % chromium),

1.1.21 Grade 35Titanium alloy (4.5 % aluminum, 2 % molybdenum, 1.6 % vanadium, 0.5 % iron, 0.3 % silicon),

1.1.22 Grade 36Titanium alloy (45 % niobium),

1.1.23 Grade 37Titanium alloy (1.5 % aluminum), and

1.1.24 Grade 38Titanium alloy (4 % aluminum, 2.5 % vanadium, 1.5 % iron).

Note 1—H grade material is identical to the corresponding numeric grade (that is, Grade 2H = Grade 2) except for the higher guaranteed minimum UTS, and may always be certified as meeting the requirements of its corresponding numeric grade. Grades 2H, 7H, 16H, and 26H are intended primarily for pressure vessel use.

The H grades were added in response to a user association request based on its study of over 5200 commercial Grade 2, 7, 16, and 26 test reports, where over 99 % met the 58 ksi minimum UTS.

1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.


2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.

ASTM Standards

A370 Test Methods and Definitions for Mechanical Testing of Steel Products
E8 Test Methods for Tension Testing of Metallic Materials
E29 Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications
E1409 Test Method for Determination of Oxygen and Nitrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique
E1447 Test Method for Determination of Hydrogen in Titanium and Titanium Alloys by Inert Gas Fusion Thermal Conductivity/Infrared Detection Method
E1941 Test Method for Determination of Carbon in Refractory and Reactive Metals and Their Alloys by Combustion Analysis
E2371 Test Method for Analysis of Titanium and Titanium Alloys by Atomic Emission Plasma Spectrometry
E2626 Guide for Spectrometric Analysis of Reactive and Refractory Metals


Keywords

seamless tubing; titanium; titanium alloy; tubing; welded/cold worked tubing; welded tubing ; Condenser and heat exchanger systems--titanium/titanium alloy; Palladium (titanium plus palladium)--specifications; Titanium alloy pipe/tube--specifications; Titanium plus palladium--specifications; Titanium (Ti)/alloys--specifications; UNS R50250 (Ti, unalloyed); UNS R50400 (Ti, unalloyed); UNS R50700 (Ti, unalloyed); UNS R52250 (Ti, low-alloyed); UNS R52400 (Ti, low-alloyed); UNS R53400 (Ti alloy); UNS R54520 (Ti alloy); UNS R56320 (Ti alloy); UNS R58030 (Ti alloy); Welded Ti/Ti alloy--specifications; UNS R50550 (Ti, unalloyed)



ICS Code

ICS Number Code 23.040.15 (Non-ferrous metal pipes)



DOI: 10.1520/B0338-10

ASTM International is a member of CrossRef.


Citing ASTM Standards

[Back to Top]

Standards Tracker

Standards Subscriptions


Users also bought:
A370
B265