ASTM A384/A384M-07

    Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies


      Format Pages Price  
    PDF 3 $45.60   ADD TO CART


    1. Scope

    1.1 Steel assemblies and subassemblies fabricated by welding, such as composite structural members, sash, weldments, etc., that are to be hot-dip galvanized after fabrication, are subject to warpage and distortion of the material due to the heating and cooling integral to the galvanizing operation, particularly when it is necessary for the assembly to be dipped more than once to coat the entire surface.

    1.2 This specification is applicable in either inch pounds or SI units. Inch pounds and SI units are not necessarily exact equivalents. Within the text of this specification and where appropriate, SI units are shown in parentheses.


    2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.

    ASTM Standards

    A143/A143M Practice for Safeguarding Against Embrittlement of Hot-Dip Galvanized Structural Steel Products and Procedure for Detecting Embrittlement

    A385 Practice for Providing High-Quality Zinc Coatings (Hot-Dip)

    A780 Practice for Repair of Damaged and Uncoated Areas of Hot-Dip Galvanized Coatings


    ICS Code

    ICS Number Code 25.220.20 (Surface treatment)

    UNSPSC Code

    UNSPSC Code 30102204(Steel plate)


    Referencing This Standard

    DOI: 10.1520/A0384_A0384M-07

    ASTM International is a member of CrossRef.


    Citation Format

    ASTM A384 / A384M-07, Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies, ASTM International, West Conshohocken, PA, 2007, www.astm.org